In a well-ventilated area, connect your aluminum to a power source and place it in a tub of a 1:1 mixture of distilled water and battery acid. Run the power to your aluminum for 45 minutes, then remove it from the tub. Place the anodized metal in a hot dye bath for 15 minutes afterward to dye. Part 1.